Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex TEKBOND® 6000-35 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name TEKBOND®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex TEKBOND® 6000-35 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Linear Mold Shrinkage 0.025 cm/cm
0.025 in/in
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 200 °C
35 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
ASTM D2240
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Users viewing this material also viewed the following: