Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM 792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
10 seconds; ASTM D2240
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Tear Strength 40.3 kN/m
230 pli
ASTM D624