Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 220 MPa | 31900 psi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ASTM D638 |
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Strength, Yield | >= 220 MPa | >= 31900 psi | |
MetalTek MTEK 70-30 UNS C96400 Nickel-Copper Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 %, Temperature 870 °C |
31900 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36XXP PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RCL36XXP is a compound based on PA 66 resin, containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ASTM D638 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: .. |
|||
Tensile Strength, Yield | 220 MPa @Temperature 550 °C |
31900 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 %, Temperature 650 °C |
31900 psi @Strain 0.200 %, Temperature 1200 °F |
Solution Annealed prior to test |
Special Metals INCONEL® Alloy 617 A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by.. |
|||
Tensile Strength, Yield | 220 - 280 MPa @Strain 0.200 % |
31900 - 40600 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 220 RP High-strength Steel High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi.. |
|||
Tensile Strength, Yield | 220 - 280 MPa @Strain 0.200 % |
31900 - 40600 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 220 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 220 - 280 MPa @Strain 0.200 % |
31900 - 40600 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 220 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | <= 220 MPa @Strain 0.200 % |
<= 31900 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal F36 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Tensile Strength, Yield | >= 220 MPa | >= 31900 psi | |
SSAB Tunnplat Domex® 220YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Tensile Strength, Yield | <= 220 MPa @Strain 0.200 %, Thickness <=0.700 mm |
<= 31900 psi @Strain 0.200 %, Thickness <=0.0276 in |
20 MPa higher apply |
SSAB Tunnplat Aluzink F36A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Tensile Strength, Yield | 220 MPa @Strain 0.200 % |
31900 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ISO 527 |
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ISO 527 |
Polyram PlusTek PB302G50BK39D Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Tensile Strength, Yield | >= 220 MPa @Strain 0.200 % |
>= 31900 psi @Strain 0.200 % |
|
CLAL-MSX CUPROROR® TL1 1/4 hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Tensile Strength, Yield | 220 - 280 MPa | 31900 - 40600 psi | |
ArcelorMittal 14 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD14) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Yield | 220 - 270 MPa | 31900 - 39200 psi | |
ArcelorMittal 220 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC220B), electroglavanized (HC220B+ZE) and Extragal®/Galvannealed (HC220BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 220 - 260 MPa | 31900 - 37700 psi | |
ArcelorMittal IF 220 High strength IF steel, Cold rolled Available in the following: uncoated (HC220Y), electroglavanized (HC220Y+ZE) and Extragal®/Galvannealed (HX220YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Yield | 220 - 280 MPa | 31900 - 40600 psi | |
ArcelorMittal H 220 Solid solution steel, Cold rolled Available in the following: uncoated (HC220P) and electrogalvanized (HC220P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Tensile Strength, Yield | 220 MPa | 31900 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |