Special Metals INCONEL® Alloy 617

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® Alloy 617.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by an aluminum addition. The alloy also resists a wide range of corrosive aqueous environments. Used in gas turbines for combustion cans, ducting, and transition liners; for petrochemical processing; for heat-treating equipment; and in nitric acid production. Standard product forms are round, forging stock, extruded section, plate, sheet, strip, pipe, tube, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 570 MPa

@Temperature 650 °C
82700 psi

@Temperature 1200 °F
Solution Annealed prior to test
710 MPa

@Temperature 23.0 °C
103000 psi

@Temperature 73.4 °F
Tensile Strength, Yield 340 MPa

@Strain 0.200 %
49300 psi

@Strain 0.200 %
Solution Annealed. Value at room temperature
220 MPa

@Strain 0.200 %,
Temperature 650 °C
31900 psi

@Strain 0.200 %,
Temperature 1200 °F
Solution Annealed prior to test
Elongation at Break 62 %
62 %
Solution Annealed
50 %

@Temperature 650 °C
50 %

@Temperature 1200 °F
Solution Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 11.6 µm/m-°C

@Temperature 20.0 - 100 °C
6.44 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.419 J/g-°C
0.100 BTU/lb-°F
Thermal Conductivity 13.6 W/m-K
94.4 BTU-in/hr-ft²-°F
Melting Point 1330 - 1380 °C
2430 - 2520 °F
Solidus 1330 °C
2430 °F
Liquidus 1380 °C
2520 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.80 - 1.5 %
0.80 - 1.5 %
Boron, B <= 0.0060 %
<= 0.0060 %
Carbon, C 0.050 - 0.15 %
0.050 - 0.15 %
Chromium, Cr 20 - 24 %
20 - 24 %
Cobalt, Co 10 - 15 %
10 - 15 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni >= 44.5 %
>= 44.5 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti <= 0.60 %
<= 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000122 ohm-cm
0.000122 ohm-cm