Polymer Property : Tensile Strength, Yield = 37700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 - 260 MPa
3600 - 37700 psi
Average value: 211 MPa Grade Count:7
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Strength, Yield 180 - 260 MPa
26100 - 37700 psi
ArcelorMittal 16 High formability steel for drawing, Hot rolled
Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru..
Tensile Strength, Yield 220 - 260 MPa
31900 - 37700 psi
ArcelorMittal IF 220 High strength IF steel, Cold rolled
Available in the following: uncoated (HC220Y), electroglavanized (HC220Y+ZE) and Extragal®/Galvannealed (HX220YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of..
Tensile Strength, Yield 140 - 260 MPa
20300 - 37700 psi
ArcelorMittal 53+AS Aluminized steel
Use: Difficult drawingInformation provided by ArcelorMittal