Polymer Property : Tensile Strength, Yield = 39200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 180 - 270 MPa
26100 - 39200 psi
Average value: 230 MPa Grade Count:3
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Tensile Strength, Yield 180 - 270 MPa
26100 - 39200 psi
ArcelorMittal 15 High formability steel for drawing, Hot rolled
Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru..
Tensile Strength, Yield 195 - 270 MPa
28300 - 39200 psi
ArcelorMittal 195 BH Bake hardening steel, Cold rolled
Description: The composition and processing of these steels are designed to promote a significant increase in yield strength during low-temperature heat treatment, particularly paint curing. Arcelor..
Tensile Strength, Yield 220 - 270 MPa
31900 - 39200 psi
ArcelorMittal 220 BH Bake hardening steel, Cold rolled
Available in the following: uncoated (HC220B), electroglavanized (HC220B+ZE) and Extragal®/Galvannealed (HC220BD+Z)Description: The composition and processing of these steels are designed to promot..