LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic olefin (TPO) resin. It has an excellent balance of properties and is designed primarily for injection molding applications. This resin is available in black only. It is not intended for food contact applications. Uses: Appliances, automotive applications, lawn and garden equipmentInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-1, -2
Tensile Modulus 0.703 GPa
102 ksi
ISO 527-1, -2
Flexural Modulus 0.660 GPa
95.7 ksi
ISO 178
Izod Impact, Notched (ISO) 94.6 kJ/m²

@Temperature 23.0 °C
45.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 24.0 J

@Temperature -30.0 °C
17.7 ft-lb

@Temperature -22.0 °F
Instrumented Peak Energy; ASTM D3763