Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 896 MPa | 130000 psi | 0.2% offset |
Niagara LaSalle e.t.d.® 150® Cold Finished Steel Bar e.t.d.® 150® is produced from AISI medium carbon 4100 series alloy steel. The heats to be used for e.t.d. 150® are controlled to contain nitrogen in quantities normally associated with steel prod.. |
|||
Tensile Strength, Yield | >= 895 MPa | >= 130000 psi | |
MetalTek J92240 14-4 PH® Precipitation Hardening Steel Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek |
|||
Tensile Strength, Yield | 896 MPa | 130000 psi | |
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel 9310 VAC-ARC is a premium quality alloy carburizing steel produced by the vacuum consumable electrode process. It has a high hardenability, high core hardness and high fatigue strength, all of which.. |
|||
Tensile Strength, Yield | 895 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 895 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 3 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 2.4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion res.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 22.0 °C |
130000 psi @Temperature 71.6 °F |
Hardened and tempered to 34 HRC |
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel Description: P-20 High Hard is an improved pre-hardened mold steel that has been specially designed for large plastic molds; Material is forged on a 5000 ton press assuring maximum deformation durin.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 22.0 °C |
130000 psi @Temperature 71.6 °F |
Hardened and tempered to 34 HRC |
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation du.. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Yield | 896 - 965 MPa @Strain 0.200 % |
130000 - 140000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS03 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 896 - 999 MPa @Strain 0.200 % |
130000 - 145000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum K12® Dual Hardness Steel This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp.. |
|||
Tensile Strength, Yield | 897 MPa | 130000 psi | 0.2% Offset |
ATI Allvac® 6-6-2 Titanium Alloy, Heat Treatment: 718°C (1325°F) Anneal Data provided by Allvac.Applications: Airframes, jet engines, rocket engine cases, nuclear reactor components, ordnance components. |
|||
Tensile Strength, Yield | 897 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization Data provided by Allvac.Applications: High performance helicopter transmission gears, components. |
|||
Tensile Strength, Yield | 896 MPa @Strain 0.200 %, Temperature 427 °C |
130000 psi @Strain 0.200 %, Temperature 801 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 895 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm.. |
|||
Tensile Strength, Yield | 897 MPa | 130000 psi | EN2597B |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel |
|||
Tensile Strength, Yield | 896 MPa | 130000 psi | |
HP Alloys Alloy 718, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Yield | >= 896 MPa @Strain 0.200 % |
>= 130000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |
|||
Tensile Strength, Yield | 895 MPa | 130000 psi | |
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy Stellite alloy 25 forms a protective oxide film during hot metal-on metal wear which prevents metal transfer and damage due to adhesion. The alloy is resistant to thermal cracking and surface fatig.. |
|||
Tensile Strength, Yield | 897 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age Data provided by Allvac.Applications: Turbine compressor blades and discs, shafts, spacers, fasteners, miscellaneous jet engine hardware; space shuttle turbo pump seals.Waspaloy is a registered trad.. |
|||
Tensile Strength, Yield | 896 MPa @Temperature 177 °C |
130000 psi @Temperature 351 °F |
Offset not given |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |