Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 896 - 999 MPa @Strain 0.200 % |
130000 - 145000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |