Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 931 - 1000 MPa @Strain 0.200 % |
135000 - 145000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 931 - 1000 MPa @Strain 0.200 % |
135000 - 145000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 910 - 1000 MPa @Strain 0.200 % |
132000 - 145000 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Yield | 896 - 999 MPa @Strain 0.200 % |
130000 - 145000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |