Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Cured Resin
1.50 g/cc
0.0542 lb/in³
Nominal Laminate
1.79 g/cc
0.0647 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 897 MPa
130000 psi
EN2597B
Tensile Modulus 68.2 GPa
9890 ksi
EN2597B
Compressive Yield Strength 852 MPa
124000 psi
EN2850B
Compressive Modulus 58.6 GPa
8500 ksi
EN2850B
Shear Modulus 4.10 GPa
595 ksi
EN6031
Shear Strength 69.2 MPa
10000 psi
ILSS; EN2563
121 MPa
17500 psi
In-Plane; EN6031
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 193 °C
379 °F
EN6032
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0297
Fiber Volume (%) 52.7
Nominal