Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® EH04 Epoxy Resin System

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® EH04 Epoxy Resin System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® EH04 is a modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides full cured parts in only 3 minutes at 138°C.Applications: Golf shafts, Bicycle components, Hockey Sticks, Arrow shafts, Fishing rods
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.0 MPa
11700 psi
Elongation at Yield 3.7 %
3.7 %
Tensile Modulus 3.45 GPa
500 ksi
Fracture Toughness 1.41 MPa-m½
1.28 ksi-in½
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 130 °C
266 °F
Processing Properties Metric English Comments
Gel Time 1.50 min

@Temperature 149 °C
1.50 min

@Temperature 300 °F
3.00 min

@Temperature 135 °C
3.00 min

@Temperature 275 °F
6.50 min

@Temperature 121 °C
6.50 min

@Temperature 250 °F
Copyright © lookpolymers.com All Rights Reserved