Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.0 MPa
11700 psi
ASTM D638
NYCOA 1047 PA 6
UL rated heat stabilized grade for applications greater than 100 deg. CInformation provided by NYCOA, Inc.
Tensile Strength, Yield 81.0 MPa
11700 psi
SABIC - Japan Method
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Tensile Strength, Yield 81.0 MPa
11700 psi
SABIC - Japan Method
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
Tensile Strength, Yield 81.0 MPa
11700 psi
SABIC - Japan Method
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific)
Tensile Strength, Yield 81.0 MPa
11700 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East)
LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su..
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp DFP22H PC
LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC..
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Tensile Strength, Yield 81.0 MPa
11700 psi
ASTM D638
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527
SABIC Innovative Plastics LNP Lubricomp DFI12E PC
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Tensile Strength, Yield 81.0 MPa

@Temperature 22.0 °C
11700 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP
SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t..
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66
LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant.
Tensile Strength, Yield 81.0 MPa
11700 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
Tensile Strength, Yield 81.0 MPa
11700 psi
50 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber.
Tensile Strength, Yield 81.0 MPa
11700 psi
50 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled.
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527 type 1 A
Solvay TECHNYL® A 216 PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert..
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS
LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber.
Tensile Strength, Yield 81.0 MPa
11700 psi
SABIC - Japan Method
SABIC Innovative Plastics NORYL EFN4230 PPE+PS (Asia Pacific)
PPE+PS high heat transparent grade
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527 type 1 A
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf..
Tensile Strength, Yield 81.0 MPa
11700 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
Tensile Strength, Yield 81.0 MPa
11700 psi
Hexcel® HexPly® EH04 Epoxy Resin System
HexPly® EH04 is a modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides full cured parts in only 3 minutes at 138°C.Appli..
Tensile Strength, Yield 81.0 MPa
11700 psi
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem..
Tensile Strength, Yield 81.0 MPa
11700 psi
dry; ISO 527-1/-2
DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR
Low Viscosity, Molding Release, 30% Glass Reinforced
Tensile Strength, Yield 81.0 MPa
11700 psi
ASTM D638
Entec Hypro™ PPH-GF20 Natural Homopolymer Polypropylene, 20% Glass Reinforced
Information provided by Entec
Tensile Strength, Yield 81.0 MPa
11700 psi
chs 0.2 in/min; ASTM D638
Diamond Polymers NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527-2
Cathay PA56 Renewable Engineering Polyamide, DAM
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr..
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527-2
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
Tensile Strength, Yield 81.0 MPa
11700 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications.