Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and semiprepreg) making it easy to process. When cured, HexPly® M36 becomes a tough composite with excellent hot/wet performance. Its low density contributes to increased weight savings, and the flexibility in curing gives potential for composite part cost savings.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.0 MPa
11700 psi
Tensile Modulus 3.50 GPa
508 ksi
Compressive Yield Strength 146 MPa
21200 psi
Poissons Ratio 0.42
0.42
Fracture Toughness 0.900 MPa-m½
0.819 ksi-in½
Shear Modulus 1.23 GPa
178 ksi
Calculated
Toughness 190 J
140 ft-lb
Per square meter
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 211 °C
412 °F
DMTA