Polymer Property : K (wear) Factor = 12.1 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp DFP22 PC
LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC
LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Dry: 0.25 m/s, 3.4 MPa (50 fpm, 500 psi); ASTM D3702
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK
LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP
LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFL26 PA 66
LNP LUBRICOMP* RFL26 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66
LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66
LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA (Asia Pacific)
LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA
LNP* LUBRICOMP* UFL36SXC is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific)
LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA
LNP* LUBRICOMP* UFL36SXQ is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15%PTFE. Added features of this material include: Wear Resistant, Heat Stabilized, Bearing Grade.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA (Asia Pacific)
LNP* Lubricomp* UFL36SXQ is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA
LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr..
K (wear) Factor 12.1 x 10-8 mm³/N-M
6.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC
LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated.