Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.50 - 9.00 kJ/m²
4.04 - 4.28 ft-lb/in²
ASTM D256
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Izod Impact, Notched (ISO) 9.00 - 9.00 kJ/m²

@Temperature -30.0 - -30.0 °C
4.28 - 4.28 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.00 kJ/m² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Izod Impact, Notched (ISO) 2.60 - 9.00 kJ/m²
1.24 - 4.28 ft-lb/in²
Average value: 6.18 kJ/m² Grade Count:20
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Izod Impact, Notched (ISO) 6.00 - 9.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.50 kJ/m² Grade Count:2
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Izod Impact, Notched (ISO) 6.00 - 9.00 kJ/m²
2.86 - 4.28 ft-lb/in²
Average value: 7.00 kJ/m² Grade Count:3
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 5.00 - 9.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 4.28 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.80 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Notched (ISO) 8.00 - 9.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 4.28 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.50 kJ/m² Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Izod Impact, Notched (ISO) 6.00 - 9.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 7.55 kJ/m² Grade Count:11
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Notched (ISO) 9.00 - 9.00 kJ/m²

@Temperature -30.0 - -30.0 °C
4.28 - 4.28 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.00 kJ/m² Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Izod Impact, Notched (ISO) 4.98 - 9.00 kJ/m²

@Temperature -40.0 - -20.0 °C
2.37 - 4.28 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 7.24 kJ/m² Grade Count:4