Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 4.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.80 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
0.857 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.41 kJ/m² Grade Count:7
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Izod Impact, Notched (ISO) 2.00 - 4.00 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.96 kJ/m² Grade Count:5
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 2.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.00 kJ/m² Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.50 kJ/m² Grade Count:1
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.56 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.67 kJ/m² Grade Count:1
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.50 kJ/m² Grade Count:2
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Izod Impact, Notched (ISO) 4.00 - 4.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 1.90 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.00 kJ/m² Grade Count:1
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched (ISO) 2.00 - 4.00 kJ/m²
0.952 - 1.90 ft-lb/in²
Average value: 3.38 kJ/m² Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Izod Impact, Notched (ISO) 4.00 - 4.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 1.90 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.00 kJ/m² Grade Count:1
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved