Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.80 - 4.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.857 - 1.90 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.41 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLG902 Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLG902L Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CMG302 Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Izod Impact, Notched (ISO) | 1.80 kJ/m² | 0.857 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |