Polymer Property : Izod Impact, Notched (ISO) = 0.857 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.80 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
0.857 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.41 kJ/m² Grade Count:7
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLG340 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLG902 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLG902L Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLG902LX Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLG960 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CMG302 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Izod Impact, Notched (ISO) 1.80 kJ/m²
0.857 ft-lb/in²
ISO 180/1A
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..