Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Product Applications: TECHNYLSTAR TM SX 216 V50 is suitable for all applications where a high rigidity is required. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 162 MPa
23500 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527 Type 1A
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %