Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 548B V15 is suitable in the automotive industry for blow-molded parts, mainly in the oil and air circuits, such as: air intake ducts, turbo to intercooler pipe, intercooler exit duct. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527 Type 1A
Elongation at Break 5.0 %
5.0 %
ISO 527 Type 1A
Tensile Modulus 3.80 GPa
551 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 21.0 kV/mm
533 kV/in
IEC 60243
Dissipation Factor 0.12
0.12
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %