Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RKN14 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RKN14 is a compound based on Nylon 66 resin containing Mineral, MOS2.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
5 mm/min; ISO 527
Elongation at Break 4.2 %
4.2 %
5 mm/min; ISO 527
Tensile Modulus 6.30 GPa
914 ksi
1 mm/min; ISO 527
Flexural Strength 111 MPa
16100 psi
2 mm/min; ISO 178
Flexural Modulus 5.00 GPa
725 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af