Polymer Property : Izod Impact, Unnotched = 16.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.801 - 8.54 J/cm
1.50 - 16.0 ft-lb/in
Average value: 5.11 J/cm Grade Count:44
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched 2.14 - 8.54 J/cm
4.00 - 16.0 ft-lb/in
Average value: 4.14 J/cm Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Izod Impact, Unnotched 3.20 - 8.54 J/cm

@Temperature -40.0 - -40.0 °C
5.99 - 16.0 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 5.00 J/cm Grade Count:4
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Izod Impact, Unnotched 3.20 - 8.54 J/cm

@Thickness 3.20 - 81.3 mm
5.99 - 16.0 ft-lb/in

@Thickness 0.126 - 3.20 in
Average value: 5.00 J/cm Grade Count:4
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Izod Impact, Unnotched 3.47 - 8.54 J/cm
6.50 - 16.0 ft-lb/in
Average value: 5.84 J/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 3.74 - 8.54 J/cm
7.00 - 16.0 ft-lb/in
Average value: 6.53 J/cm Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Izod Impact, Unnotched 6.41 - 8.54 J/cm
12.0 - 16.0 ft-lb/in
Average value: 7.35 J/cm Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Izod Impact, Unnotched 2.67 - 8.54 J/cm
5.00 - 16.0 ft-lb/in
Average value: 5.49 J/cm Grade Count:21
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Izod Impact, Unnotched 0.747 - 8.54 J/cm
1.40 - 16.0 ft-lb/in
Average value: 4.35 J/cm Grade Count:79
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Unnotched 1.60 - 8.54 J/cm
3.00 - 16.0 ft-lb/in
Average value: 5.23 J/cm Grade Count:73
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..