Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Carbon Fiber Filled
Manufacturer Westlake Plastics
Trade Name Pomalux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 320F. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Water Absorption 0.22 %
0.22 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 98.6 MPa
14300 psi
ASTM D790
Flexural Modulus 8.446 GPa
1225 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
Dry; ASTM D257
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B