Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.87 - 8.81 J/cm
3.50 - 16.5 ft-lb/in
Average value: 5.96 J/cm Grade Count:6
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..