Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 10.7 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.801 - 10.7 J/cm
1.50 - 20.0 ft-lb/in
Average value: 3.62 J/cm Grade Count:22
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Unnotched 2.67 - 10.7 J/cm
5.00 - 20.0 ft-lb/in
Average value: 7.12 J/cm Grade Count:6
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 7.47 J/cm Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 7.47 J/cm Grade Count:19
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Unnotched 6.41 - 10.7 J/cm
12.0 - 20.0 ft-lb/in
Average value: 8.45 J/cm Grade Count:13
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Izod Impact, Unnotched 3.20 - 10.7 J/cm
6.00 - 20.0 ft-lb/in
Average value: 6.85 J/cm Grade Count:45
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 8.33 J/cm Grade Count:15
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Izod Impact, Unnotched 3.79 - 10.7 J/cm
7.10 - 20.0 ft-lb/in
Average value: 7.37 J/cm Grade Count:10
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 2.40 - 10.7 J/cm
4.50 - 20.0 ft-lb/in
Average value: 6.27 J/cm Grade Count:31
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
Average value: 8.12 J/cm Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Unnotched 1.10 - 10.7 J/cm
2.06 - 20.0 ft-lb/in
Average value: 6.54 J/cm Grade Count:14
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 2.14 - 10.7 J/cm
4.00 - 20.0 ft-lb/in
Average value: 6.83 J/cm Grade Count:5
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Izod Impact, Unnotched 1.87 - 10.7 J/cm
3.50 - 20.0 ft-lb/in
Average value: 4.43 J/cm Grade Count:13
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched 2.14 - 10.7 J/cm
4.00 - 20.0 ft-lb/in
Average value: 5.31 J/cm Grade Count:21
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 6.43 J/cm Grade Count:22
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Izod Impact, Unnotched 8.01 - 10.7 J/cm
15.0 - 20.0 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1200-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa..
Izod Impact, Unnotched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
Average value: 7.48 J/cm Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..