Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.70 - 7.00 J/cm²
22.4 - 33.3 ft-lb/in²
Average value: 5.88 J/cm² Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Charpy Impact Unnotched 2.20 - 7.00 J/cm²
10.5 - 33.3 ft-lb/in²
Average value: 5.51 J/cm² Grade Count:17
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Charpy Impact Unnotched 2.00 - 7.00 J/cm²
9.52 - 33.3 ft-lb/in²
Average value: 4.04 J/cm² Grade Count:13
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Charpy Impact Unnotched 2.50 - 7.00 J/cm²

@Temperature -40.0 - 30.0 °C
11.9 - 33.3 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 4.64 J/cm² Grade Count:11
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Charpy Impact Unnotched 3.50 - 7.00 J/cm²
16.7 - 33.3 ft-lb/in²
Average value: 5.62 J/cm² Grade Count:13
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 3.00 - 7.00 J/cm²

@Temperature -20.0 - 30.0 °C
14.3 - 33.3 ft-lb/in²

@Temperature -4.00 - 86.0 °F
Average value: 4.40 J/cm² Grade Count:5
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 2.30 - 7.00 J/cm²
10.9 - 33.3 ft-lb/in²
Average value: 4.54 J/cm² Grade Count:41
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.00 - 7.00 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.27 J/cm² Grade Count:34
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.70 - 7.00 J/cm²
12.8 - 33.3 ft-lb/in²
Average value: 4.88 J/cm² Grade Count:13
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Charpy Impact Unnotched 2.30 - 7.00 J/cm²
10.9 - 33.3 ft-lb/in²
Average value: 4.49 J/cm² Grade Count:27
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..