Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 2-8302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8302 is developed for extrusion of sheets, profiles and for blow molding of different bottles.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.900 g/cc

@Temperature 23.0 °C
0.0325 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 20 %
20 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 0.850 GPa
123 ksi
1 mm/min; ISO 527-1,-2
Flexural Modulus 1.00 GPa
145 ksi
2 mm/min; ISO 178
Charpy Impact, Notched 3.00 J/cm²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1,-2
Descriptive Properties Value Comments
Color Natural