Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Solvay TECHNYL® eXten D 458P PA6.10, Conditioned Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |