Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinelec CCB6814 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Teknor Apex Company
Trade Name Sinelec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinelec CCB6814 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Melt Flow 0.500 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.500 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 64 %
64 %
ASTM D638
Flexural Strength 35.0 MPa
5080 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 1.71 J/cm

@Temperature 22.8 °C
3.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
Loading 1 (10N); ASTM D1525
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257