Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0055 - 0.010 cm/cm
0.0055 - 0.010 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Ash 30 - 35 %
30 - 35 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.365 MPa
53.0 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Strength 0.538 MPa
78.0 psi
ASTM D790
Flexural Modulus 0.0269 GPa
3.90 ksi
1% Secant; ASTM D790
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
268 °F
Unannealed; ASTM D648
Flame Spread <= 100 mm/min
<= 3.94 in/min
ISO 3795
Descriptive Properties Value Comments
Impact Change, % Max 25
ISO 180
Tensile Change, % Max 25
ISO R527