Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 - 0.854 J/cm | 1.00 - 1.60 ft-lb/in | Average value: 0.725 J/cm Grade Count:14 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.267 - 0.854 J/cm | 0.500 - 1.60 ft-lb/in | Average value: 0.483 J/cm Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.320 - 0.854 J/cm | 0.600 - 1.60 ft-lb/in | Average value: 0.687 J/cm Grade Count:41 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 0.160 - 0.854 J/cm | 0.300 - 1.60 ft-lb/in | Average value: 0.344 J/cm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.534 - 0.854 J/cm | 1.00 - 1.60 ft-lb/in | Average value: 0.667 J/cm Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.534 - 0.854 J/cm | 1.00 - 1.60 ft-lb/in | Average value: 0.667 J/cm Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.320 - 0.854 J/cm | 0.600 - 1.60 ft-lb/in | Average value: 0.672 J/cm Grade Count:22 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |