Material Notes:
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.Nov. 2009: Veradel® is the replacement trade name for former Radel® R PESU products.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.42 %
0.42 %
in 24 hours per ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 126 MPa
18300 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Elongation at Yield 1.9 %
1.9 %
ASTM D638
Tensile Modulus 8.62 GPa
1250 ksi
ASTM D638
Flexural Yield Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 8.07 GPa
1170 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Tensile Impact Strength 70.0 kJ/m²
33.3 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
CTE, linear, Transverse to Flow 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F
ASTM D648
UL RTI, Electrical 190 °C

@Thickness 1.57 mm
374 °F

@Thickness 0.0618 in
UL RTI, Mechanical with Impact 190 °C

@Thickness 1.57 mm
374 °F

@Thickness 0.0618 in
UL RTI, Mechanical without Impact 190 °C

@Thickness 1.57 mm
374 °F

@Thickness 0.0618 in
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.1

@Frequency 1000 Hz
4.1

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm

@Thickness 3.30 mm
457 kV/in

@Thickness 0.130 in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150