Reliance Industries Repol B120MA Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol B120MA Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene B120MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol B120MA is recommended for use in injection molding processes where medium impact strength is required. It is an ideal material for housewares, thermowares, sanitarywares, furniture, industrial and automotive components. Repol B120MA contains antistatic agent that reduces static charge build up on products. Features:High flow behaviorGood stiffness-impact balanceGood surface glossLow static charge build up and reduced dust pickupInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50mm/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Users viewing this material also viewed the following: