Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 102 MPa
14800 psi
ASTM D790
Flexural Modulus 3.87 GPa
561 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ASTM D648