Material Notes:
A general purpose basic Nylon 66 resin, slightly lubricated.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ATSM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1e+6 Hz
3.9

@Frequency 1e+6 Hz
ASTM D150