Material Notes:
LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
4.0 %
4.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.89 GPa
419 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
96.0 MPa
13900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
2.82 GPa
409 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.68 J/cm
20.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 3.20 mm
250 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257