Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH  (d

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH  (d.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent dimensional stability and low moisture absorption. There are two versions of AMODEL A-1240 resin, "L" and "HS". The L version will usually provide the smoother, higher gloss surface, while the HS version gives better long-term thermal aging properties. Both AMODEL A-1240 resins can be easily processed using conventional equipment and methods.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material dry as molded.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Dry As Molded
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM E831
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ASTM E831
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.0 MPa
13500 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ASTM D638
Tensile Modulus 8.30 GPa
1200 ksi
ASTM D638
Flexural Yield Strength 176 MPa
25500 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Shear Strength 93.0 MPa
13500 psi
ASTM D732
Izod Impact, Notched 0.310 J/cm
0.581 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
ASTM D150
4.4

@Frequency 100 Hz
4.4

@Frequency 100 Hz
ASTM D150
Dissipation Factor 0.0070

@Frequency 100 Hz
0.0070

@Frequency 100 Hz
ASTM D150
0.019

@Frequency 1e+6 Hz
0.019

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 550 V
550 V
Processing Properties Metric English Comments
Melt Temperature 321 - 343 °C
610 - 649 °F
Injection