Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.520 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.974 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature -30.0 °C |
0.974 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
Izod Impact, Notched | >= 0.520 J/cm @Temperature 23.0 °C |
>= 0.974 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 4052U (52411) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 0.520 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.974 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedNon-HalogenatedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
Izod Impact, Notched | 0.520 - 0.520 J/cm @Temperature -40.0 - -40.0 °C |
0.974 - 0.974 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.520 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature 23.0 °C |
0.974 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Izod Impact, Notched | >= 0.520 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.974 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Izod Impact, Notched | 0.520 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.974 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2156FM PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature -40.0 °C |
0.974 ft-lb/in @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ ETA-3104HF Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color.. |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature 23.0 °C |
0.974 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature 0.000 °C |
0.974 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant Applications: Lamp partsHome electric appliance partsFeatures: Fine appearanceHigh rigidityImpact resistantInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.520 J/cm @Temperature -40.0 °C |
0.974 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman PROVISTA Copolymer PETG Copolyester Color, b* CIELAB, Illuminant D6500, 10° Observer is 0.61 per ASTM D 2244.Product Description: PROVISTA Copolymer is a resin specifically developed for extrusion into profiles where aesthetics like.. |
|||
Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |