Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC PP 510P Polypropylene Homopolymer for Fiber Applications Product Description: PP 510P is a homopolymer specially designed for fiber extrusion applications with the following features:Consistent processabilityGood thread line stabilityGood color consisten.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC PP 511A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 511A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 511A has the following features:Consis.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC PP 575P Polypropylene Homopolymer for Injection Molding Product Description: PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -30.0 °C |
0.412 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Izod Impact, Notched | 0.220 - 5.88 J/cm | 0.412 - 11.0 ft-lb/in | Average value: 2.91 J/cm Grade Count:145 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -30.0 °C |
0.412 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ EP 5001C(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature 23.0 °C |
0.412 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 - 0.260 J/cm | 0.412 - 0.487 ft-lb/in | ASTM D256A |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3 Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Izod Impact, Notched | 0.220 - 0.390 J/cm | 0.412 - 0.731 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Izod Impact, Notched | 0.220 J/cm @Thickness 3.20 mm |
0.412 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® GL1200 ABS General Purpose Grade Middle impact, Good mechanical strength, High flexural strengthInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |
|||
Izod Impact, Notched | 0.220 - 0.801 J/cm | 0.412 - 1.50 ft-lb/in | Average value: 0.471 J/cm Grade Count:18 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |