Material Notes:
Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Suggested fabrication methods: Injection molding; Extrusion; ThermoformingFeatures: High tenacityTypical applications: Strapping, NettingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.59 GPa
231 ksi
ASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm

@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Thermoforming