Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 HS-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DIN 53453 |
Nilit RECONYL B S20 Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® M201AS Increased chemical resistance compared to P2x, contains antistatic additives.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene BL8 (HM 7745) is a high density polyethylene with Butene-1 as comonomer.Applications: for heating oil storage tanks, large containers for various chemicals.Information provided by Iran Petrochemical.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179-1 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Ductile Failure; ASTM D256B |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-5H PA12-GF50 Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SM-2 PTFE Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |