Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatures as well as easy processing. AKROMID® A is an engineering plastic compound that allows a broad range of possible applications. On the basis of these standard types, we are able to develop individual compounds for special application needs.Information from Akro-Plastic
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISOv1183
Filler Content 35 %
35 %
ISO 1172
Water Absorption 1.8 - 2.0 %

@Temperature 70.0 °C
1.8 - 2.0 %

@Temperature 158 °F
62% r.h., Humidity; ISO 62
Water Absorption at Saturation 4.7 - 5.3 %

@Time 82800 sec
4.7 - 5.3 %

@Time 23.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0017 cm/cm
0.0017 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
5 [mm/min]; ISO 527-1/2
Elongation at Break 5.0 %
5.0 %
5 [mm/min]; ISO 527-1/2
Tensile Modulus 8.40 GPa
1220 ksi
1[mm/min]; ISO 527-1/2
Flexural Strength 245 MPa
35500 psi
2 [mm/min]; ISO 178
Flexural Modulus 8.00 GPa
1160 ksi
2 [mm/min]; ISO 178
Charpy Impact Unnotched 10.2 J/cm²

@Temperature 23.0 °C
48.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357-1/3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093