SABIC Innovative Plastics SABIC STAMAX 30YM243 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name SABIC STAMAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics SABIC STAMAX 30YM243 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 209768303.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Filler Content 30 %
30 %
glass; ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.0 MPa
14100 psi
Type I, 50 mm/min; ASTM D638
110 MPa
16000 psi
50 mm/min, 1A; ISO 527
51.0 MPa

@Temperature 120 °C
7400 psi

@Temperature 248 °F
50 mm/min, 1A; ISO 527
70.0 MPa

@Temperature 80.0 °C
10200 psi

@Temperature 176 °F
50 mm/min, 1A; ISO 527
Elongation at Break 2.0 %
2.0 %
Type I, 50 mm/min; ASTM D638
2.3 %
2.3 %
50 mm/min; ISO 527
Tensile Modulus 6.65 GPa
965 ksi
1 mm/min; ISO 527
6.69 GPa
970 ksi
50 mm/min; ASTM D638
3.50 GPa

@Temperature 120 °C
508 ksi

@Temperature 248 °F
1 mm/min; ISO 527
4.60 GPa

@Temperature 80.0 °C
667 ksi

@Temperature 176 °F
1 mm/min; ISO 527
Flexural Modulus 5.79 GPa
840 ksi
1.3 mm/min, 50 mm span; ASTM D790
5.90 GPa
856 ksi
2 mm/min, 64mm span; ISO 178
4.20 GPa

@Temperature 80.0 °C
609 ksi

@Temperature 176 °F
2 mm/min, 64mm span; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
80*10*4mm, Cut; ISO 75-1&2
158 °C

@Thickness 3.20 mm
316 °F

@Thickness 0.126 in
ASTM D648