Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America Product Applications: Due to its outstanding flow characteristics, TECHNYL STAR S 218 V35 BLACK 31N provides a significant productivity improvement and allows more freedom in mould design and part design versus standard polyamide solutions. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527 Type 1A
Elongation at Break 4.5 %
4.5 %
ISO 527 Type 1A
Tensile Modulus 7.40 GPa
1070 ksi
ISO 527 Type 1A
Flexural Strength 195 MPa
28300 psi
ISO 178
Flexural Modulus 6.20 GPa
899 ksi
ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %