Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.850 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Radici Radilon® AUSX200 (dry) Nylon 66
Very high impact strengthInformation provided by Radici group.
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese Celanex® 4300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.30% glass fiber, good impact strength, laser markableInformation provided by Celanese
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Celcon® M50 POM  (Unverified Data**)
Celcon® M50 is a extrusion and injection molding grade with an intermediate viscosity for good processability with higher toughness than general purpose grades.Standard extruders with a length to d..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Hostaform® C 2521 XAP² ™ POM  (Unverified Data**)
POM copolymerlow EmissionInformation provided by Celanese
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
LATI Lastilac MR MDT05-01 ABS
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Magnetic detectable filler. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North ..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF)
Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7100-15 Polycarbonate
CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7102-15 Polycarbonate
CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7103-15 Polycarbonate
CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 217 PA66, Conditioned
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
IS0179
Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Borealis Bormod™ BF970MO Polypropylene for Injection Molding
Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)  (Unverified Data**)
Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese CELANEX 4300FC PBT, 30% Glass Reinforced
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.Information provided by Celanese
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese FORTRON 1342L4 PPS, 40% Specialty
Fortron 1342L4 is a low wear grade, ideally suited for bearings, gears and other sliding friction/wear applications. This product is glass fiber reinforced and contains PTFE.Information provided by ..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Hostaform® C 2521 LS POM, UV Resistant
Information provided by Celanese
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Hostaform® C 2521 XAP² ™ POM, Unfilled
POM copolymerInformation provided by Celanese
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese Hostaform® M15HP POM, Unfilled
Hostaform« acetal copolymer grade M15HP is a high viscosity polymerInformation provided by Celanese
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned)
Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Celcon® M50 POM, Unfilled
Celcon« M50 is a extrusion and injection molding grade with an intermediate viscosity for good processability with higher toughness than general purpose grades.Information provided by Celanese
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Hostaform® M25AE POM, Unfilled
Hostaform« M25AE is a special grade of acetal copolymer targeted for extrusion shapes (rod, bar, plate, etc) free of center porosity in large diameters and thicknesses.Information provided by Celan..
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Copyright © lookpolymers.com All Rights Reserved