Material Notes:
CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTTLES
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 85 hour
>= 85 hour
Condition B, F50; ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
DIN 53505
Tensile Strength at Break 36.5 MPa
5290 psi
ASTM D638
Tensile Strength, Yield 31.5 MPa
4570 psi
ASTM D638
Elongation at Break 2050 %
2050 %
ASTM D638
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 170 - 200 °C
338 - 392 °F