Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eU
Total Lacqrene® 3351(EU) Impact Polystyrene  (discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.05 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 358-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
DIN 53453
IRPC Polimaxx Polene GM2860 High Density Polyethylene
CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7100-15 Polycarbonate
CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7101-15 Polycarbonate
CALIBREâ„¢ 7101-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7102-15 Polycarbonate
CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Styron CALIBREâ„¢ 7103-15 Polycarbonate
CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
IS0179
Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
IS0179
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Borealis Bormod™ BF970MO Polypropylene for Injection Molding
Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -20.0 °C
4.05 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
Charpy Impact, Notched 0.850 J/cm²

@Temperature -30.0 °C
4.05 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Petra® 130 BK-112 30% Glass Filled PET
Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength ..
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned)
Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good..
Charpy Impact, Notched 0.850 - 1.60 J/cm²
4.05 - 7.61 ft-lb/in²
Average value: 1.06 J/cm² Grade Count:14
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Charpy Impact, Notched 0.850 J/cm²

@Temperature 23.0 °C
4.05 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 179/1eA
SYNTHOS Krasten® 552M High Impact Polystyrene
High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i..