Material Notes:
CHARACTERISTICS: EXCELLENT HIGH STIFFNESS, HEAT STABILITY, HIGH FLOW CONTAIN LONG TERM HEAT AGING ADDITIVE APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, COFFEE MAKER, HAIR DRYER
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Yield 22 %
22 %
ASTM D638
Flexural Modulus 1.85 GPa
268 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.230 J/cm²

@Temperature 23.0 °C
1.09 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 129 °C
264 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 190 - 240 °C
374 - 464 °F