Polymer Property : Ball Indentation Hardness = 210 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 210 MPa
30500 psi
ISO 2039-1
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data)
Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black..
Ball Indentation Hardness 210 MPa
30500 psi
ISO2039.1 DIN.53456
Omnia Plastica PA6 GF Akulon GF - Dry
Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-30 PA6-GF30
Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-30 S PA6-GF30
Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-30/2 PA6-GF30
Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15
Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65
Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following ..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45
Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon ..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30 PA666-GF30
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30
Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30
Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Ball Indentation Hardness 210 MPa
30500 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30
Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4104 nat PA610-GF40
Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010..
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl..
Ball Indentation Hardness 210 MPa
30500 psi
Measured by nanoindentation
Dow SiLK™ D Semiconductor Dielectric Resin
SiLK™ D resin provides a more controlled coefficient of thermal expansion (CTE) profile at elevated temperatures as compared to earlier versions of SiLK™ resin.Information provided by Dow
Ball Indentation Hardness 210 MPa
30500 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-50 HM PA6-GF50
Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop..
Ball Indentation Hardness 210 MPa
30500 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30
Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation ..
Ball Indentation Hardness 210 MPa

@Load 36.5 kg
30500 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Ball Indentation Hardness 210 MPa

@Load 36.5 kg
30500 psi

@Load 80.5 lb
dry; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced
35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Ball Indentation Hardness 210 MPa
30500 psi
H961/30; ISO 2039-1
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Ball Indentation Hardness 210 MPa

@Load 36.5 kg
30500 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..